Separation efficiencies of hollow glass beads were measured under room temperature and different nozzle inlet total pressures from 482 kPa to 537 kPa.
建立了超音速气固两相分离装置试验系统,在室温和不同喷管进口全压下,对空心玻璃珠颗粒的分离效率进行了试验研究。
The Cause of aberration in glass block producing process is analysedthe methed of improving the white degree of the glass block and keeping their color stabilization are also discussed sed.
本文就玻璃空心砖生产过程中产生色差的原因进行了分析 ,并就如何提高玻璃空心砖的白度并保持颜色稳定进行了探
Regular maintenance of molds is an important measure to improve the surface quality of hollow glass blocks.
本文主要介绍了空心玻璃砖的生产工艺及生产中注意的问题,讨论了空心玻璃砖的主要缺陷及解决办法,指出模具定期维修也是保证玻璃砖表面质量的重要措施。