Composite oxide powders of α Fe 2O 3 K 2O B 2O 3 were synthesized by stearic acid gel method, and the porous ceramic materials were detained by the liquid phase calcination method.
用硬脂酸凝胶法工艺合成不同配比的α Fe2 O3 K2 O B2 O3复合氧化物超微粉 ,经液相烧结法制得多孔陶瓷材料 。
Nanocrystals Y 2O 3 were prepared by the stearic acid gel method.
采用硬脂酸凝胶法制备了 Y2 O3纳米晶 ,用傅立叶变换红外光谱 ( FTIR) ,热重 -差热 ( TG- DTA)对制备过程进行了表征。
BaTiO3 ultrafine powder is prepared by the stearic acid gel method.
用硬脂酸凝胶法制备了BaTiO_3超微粉。