Effects of electrochemical deposition of zinc-oxides and/or zinc-hydroxides on sintered nickel electrode;
预先电沉积ZnO/Zn(OH)_2对烧结镍电极的影响
Effect of deposition layer cerium-oxides(+4) on sintered nickel electrode was studied.
在烧结镍基体表面,预先电沉积一层氧化铈,通过电化浸渍得到镍电极,研究了预先电沉积氧化铈对烧结镍电极性能的影响。
The porosity of the electrode current collector and the utility of the active materials were increased by adjusting the electrode manufacturing parameters of sintered Ni electrode and parted electrode.
通过改进、调整烧结镍电极及涂膏金属氢化物电极生产工艺参数 ,提高了电极基板孔率及活性物质利用率 ,使烧结镍电极体积比容量达到 5 40mAh/cm3 ,金属氢化物电极体积比容量达到 115 0mAh/cm3 。
With the specific capacity of the sintered Ni electrode and pasted Cd electrode increa sing by 35% and 27% respectively as well as the partition connecting method adopted, which is reliable and convenient, the battery 5GNFG150 has reached the performance indexes of nominal capacity 150Ah, nominal voltage 6V, and energy density 50Wh/kg.
通过提高烧结镍电极和涂膏镉电极的质量比容量(分别提高了35%和27%),并采用穿壁联接结构(联接良好,操作简单),使研制的5GNFG150电池组达到了额定容量150Ah,标称电压6V,质量比能量50Wh/kg以上的技术指标要求。